Microstructure evolution of magnetite layer on CLAM steel exposed to lead-bismuth eutectic containing 10(-6) wt% oxygen at 500 & DEG;C

期刊论文

JOURNAL OF NUCLEAR MATERIALS, 2022, 卷号: 562
作者:  Luo, Lin;  Liu, Jing;  Tian, Shujian;  Jiang, Zhizhong;  Xiao, Zunqi;  Zhang, Min;  Huang, Wangli;  Sun, Lujun;  Luo, Wenwei
收藏  |  浏览/下载:37/0  |  提交时间:2022/12/23
CLAM  Lead-bismuth eutectic  Magnetite  Island growth  Microstructure evolution  
Evolution of creep behavior of CLAM steel after thermal aging at 550 degrees C 期刊论文
JOURNAL OF NUCLEAR MATERIALS, 2018, 卷号: 510, 期号: 无, 页码: 265-269
作者:  Wang, Wei;  Xu, Gang;  He, Kaihui
Adobe PDF(1512Kb)  |  收藏  |  浏览/下载:111/39  |  提交时间:2019/12/25
CLAM steel  Thermal aging  Creep deformation behavior  
Effect of tempering time on fatigue crack growth behavior of CLAM steel 期刊论文
JOURNAL OF NUCLEAR MATERIALS, 2018, 卷号: 510, 页码: 437-445
作者:  Liang, Mengtian;  Zhao, Yanyun;  Zheng, Mingjie;  Mao, Xiaodong
收藏  |  浏览/下载:31/0  |  提交时间:2019/12/25
CLAM steel  Fatigue crack growth  Tempering time  Martensitic laths  Precipitates  
Experimental and numerical simulation analysis on creep crack growth behavior of CLAM steel 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 卷号: 735, 期号: 无, 页码: 260-268
作者:  Zhao, Y.;  Liu, S.;  Shi, J.;  Mao, X.
浏览  |  Adobe PDF(2681Kb)  |  收藏  |  浏览/下载:94/37  |  提交时间:2019/12/25
Creep crack growth  C* parameter  Microstructure evolution  CLAM steel  
Erosion and deuterium retention of CLF-1 steel exposed to deuterium plasma 期刊论文
PHYSICA SCRIPTA, 2017, 卷号: T170, 期号: 无, 页码: 8
作者:  Qiao, L.;  Wang, P.;  Hu, M.;  Gao, L.;  Jacob, W.;  Fu, E. G.;  Luo, G. N.
浏览  |  Adobe PDF(3630Kb)  |  收藏  |  浏览/下载:97/41  |  提交时间:2019/06/17
deuterium retention  erosion  CLF-1 steel  deuterium plasma  sputtering yield  
Status and improvement of CLAM for nuclear application 期刊论文
NUCLEAR FUSION, 2017, 卷号: 57, 期号: 8, 页码: 1-10
作者:  Huang, Qunying
浏览  |  Adobe PDF(3226Kb)  |  收藏  |  浏览/下载:133/48  |  提交时间:2018/07/27
Clam  Test Blanket Module  Fusion  Iter  
550℃真空下CLAM钢蠕变-疲劳行为及失效机理研究 学位论文
, 合肥: 中国科学技术大学, 2017
作者:  翟向伟
Adobe PDF(12524Kb)  |  收藏  |  浏览/下载:40/0  |  提交时间:2018/01/17
Surface modification of F82H steel exposed to low energy, high flux He plasmas 期刊论文
NUCLEAR FUSION, 2017, 卷号: 57, 期号: 5, 页码: 无
作者:  Xu, Yu-Ping;  Zhou, Hai-Shan;  Peng, Y. K. Martin;  Lu, Tao;  Li, Xiao-Chun;  Liu, Feng;  Wang, Jing;  Liu, Hao-Dong;  Lyu, Yi-Ming;  Luo, Guang-Nan
浏览  |  Adobe PDF(5777Kb)  |  收藏  |  浏览/下载:77/36  |  提交时间:2018/05/17
Plasma-surface Interaction  Nanostructured Layers  Rafm Steels  Helium  
Effect of thermal aging on grain structural characteristic and Ductile-to-Brittle transition temperature of CLAM steel at 550 degrees C 期刊论文
FUSION ENGINEERING AND DESIGN, 2017, 卷号: 115, 期号: 无, 页码: 74-79
作者:  Wang, Wei;  Chen, Jianwei;  Xu, Gang
浏览  |  Adobe PDF(4382Kb)  |  收藏  |  浏览/下载:116/47  |  提交时间:2018/05/04
Clam Steel  Grain Structure  Misorientation Angle  Impact Toughness  
Effect of Tantalum content on the low cycle fatigue properties of CLAM steel at 823 K 期刊论文
FUSION ENGINEERING AND DESIGN, 2017, 卷号: 114, 期号: 无, 页码: 211-218
作者:  Zhai, Xiangwei;  Liu, Shaojun;  Zhao, Yanyun;  Wang, Kun
浏览  |  Adobe PDF(6401Kb)  |  收藏  |  浏览/下载:93/47  |  提交时间:2018/05/02
Clam Steel  Ta Content  Ta-rich Mx Particle  Low Cycle Fatigue Properties